GATE Civil: Concrete Structures (limit state design, RC beams, shear, slabs, columns, prestressed concrete), previous-year questions solved
Every concrete structures question from the ten official GATE Civil papers of 2022-2026 (CE1 and CE2 each year): 25 questions (11 NAT, 11 MCQ, 3 MSQ) on limit state concepts, RC beams, shear and torsion, slabs, columns and prestressed concrete, each solved to IS 456:2000 and checked by a script against the official key. GATE 2027 drops prestressed concrete (its 4 questions are marked) and adds isolated footing design, which none of these papers asked.
Questions from the ten official GATE CE papers, sessions CE1 and CE2 of GATE 2022 (IIT Kharagpur), 2023 (IIT Kanpur), 2024 (IISc Bengaluru), 2025 (IIT Roorkee) and 2026 (IIT Guwahati); solutions by Skill-Lync. · Updated 17 Nov 2026 · 12 of 25 questions on this page
In the elastic theory of reinforced concrete, how is the modular ratio defined?
In the context of elastic theory of reinforced concrete, the modular ratio is defined as the ratio of
- (A)Young’s modulus of elasticity of reinforcement material to Young’s modulus of elasticity of concrete.
- (B)Young’s modulus of elasticity of concrete to Young’s modulus of elasticity of reinforcement material.
- (C)shear modulus of reinforcement material to the shear modulus of concrete.
- (D)Young’s modulus of elasticity of reinforcement material to the shear modulus of concrete.
Answer: (A) Young’s modulus of reinforcement to Young’s modulus of concrete Official key: A
- Working stress (elastic) theory assumes plane sections stay plane and both materials stay elastic and perfectly bonded, so the steel strain equals the surrounding concrete strain: .
- Then , so . The factor that converts steel into an equivalent area of concrete is , the modular ratio.
- It is a ratio of Young's moduli because the transformed section is built for axial/bending strain, not shear strain. IS 456 Annex B-1.3(d) gives ; for M20, (Table 21), so , a number well above 1, as steel is much stiffer than concrete.
- Answer: (A)
Trap: (B) is the reciprocal, which would be less than 1 and would shrink the steel instead of magnifying it. The code formula already allows for creep, so it gives a larger than .
Transformed-section properties with the modular ratio are still used in design offices for crack-width and deflection checks under service loads, and for checking water-retaining structures to IS 3370, where working stress design remains the governing method.
What does M20 concrete mean as per IS 456: average or 5-percentile, cube or cylinder strength?
M20 concrete as per IS 456: 2000 refers to concrete with a design mix having ________
- (A)an average cube strength of 20 MPa
- (B)an average cylinder strength of 20 MPa
- (C)a 5-percentile cube strength of 20 MPa
- (D)a 5-percentile cylinder strength of 20 MPa
Answer: (C) a 5-percentile cube strength of 20 MPa Official key: C
- IS 456 Cl. 6.1 and Table 2: in the grade designation M20, the number is the characteristic compressive strength of 150 mm cubes at 28 days, in N/mm2. So the specimen is a cube, not a cylinder.
- Characteristic strength (IS 456 Cl. 36.1) is the strength below which not more than 5 % of test results are expected to fall, i.e. the 5-percentile value. It is the starting value of limit state design, which then divides by the partial safety factor .
- The average is higher: with the IS 10262 assumed standard deviation for M20, the mix must target so that only 5 % of cubes fall below 20.
- Answer: (C) a 5-percentile cube strength of 20 MPa
Trap: (A). A mix whose average cube strength is only 20 MPa would have half its cubes below 20 MPa. (D) describes the Eurocode-style cylinder grade, which is about 0.8 times the cube value.
Ready-mix plants proportion an M20 order for a target mean near 26.6 MPa, and the site engineer judges the 28-day cube register against the IS 456 Cl. 16 acceptance criteria, not against a 20 MPa average.
Which structural design method does not apply safety factors to the design loads?
The structural design method that DOES NOT take into account the safety factors on the design loads is
- (A)working stress method.
- (B)load factor method.
- (C)ultimate load method.
- (D)limit state method.
Answer: (A) working stress method Official key: A
- Working stress method: loads are taken at their service values (). The safety lives only in the materials, through permissible stresses such as for concrete (IS 456 Annex B) and in bending for steel.
- Load factor method and ultimate load method: the working load is multiplied by a load factor and the section is designed for its ultimate strength.
- Limit state method: partial safety factors on both sides, on DL + LL (IS 456 Table 18) and for concrete, for steel (IS 456 Cl. 36.4.2).
Answer: (A) working stress method.
Trap: thinking WSM has no factor of safety at all. It does, but on the stresses, not on the loads. The question asks only about the loads.
Water-retaining structures (IS 3370) and many older bridge and steel checks are still done by working stress, so a design office keeps two load-combination sets in STAAD.Pro: unfactored service combinations for WSM and factored 1.5(DL+LL) combinations for limit state design.
Limit state of collapse design moment: 250 × 600 mm beam, 6.23 m span, 5 kN/m live + 5 kN/m dead load
A simply-supported rectangular reinforced concrete beam has a width 250 mm and an overall depth 600 mm. The effective span of the beam is 6.23 m. The beam carries a live load of 5 kN/m and super imposed dead load of 5 kN/m, in addition to its own weight. The unit weight of reinforced concrete is 25 kN/m3. Consider the load factor of 1.5 for all stated loads.
The design bending moment (in kN-m) for the limit state of collapse is ______ (rounded off to two decimal places).
Answer: Official key: 98.00 to 102.00
- The limit state of collapse is checked with factored loads: every characteristic load is multiplied by its partial safety factor before the moment is found. The beam\'s own weight is a dead load and must be included. Self-weight, using the overall depth: .
- Total service load: . Factored load (IS 456 Table 18, for DL + LL): .
- Simply supported over the effective span given (IS 456 Cl. 22.2), the moment peaks at midspan: .
- Answer: .
Trap: leaving out the self-weight gives . For a deep beam the self-weight is over a quarter of the total load here.
Every beam in an ETABS or STAAD.Pro model starts from the 1.5(DL + LL) combination with self-weight added automatically; in hand checks and spreadsheet designs a missed self-weight is one of the most common errors a checking engineer finds.
True or false: failure of over-reinforced, under-reinforced and balanced RC beam sections in flexure
Read the following statements relating to flexure of reinforced concrete beams:
I. In over-reinforced sections, the failure strain in concrete reaches earlier than the yield strain in steel.
II. In under-reinforced sections, steel reaches yielding at a load lower than the load at which the concrete reaches failure strain.
III. Over-reinforced beams are recommended in practice as compared to the under-reinforced beams.
IV. In balanced sections, the concrete reaches failure strain earlier than the yield strain in tensile steel.
Each of the above statements is either True or False.
Which one of the following combinations is correct?
- (A)I (True), II (True), III (False), IV (False)
- (B)I (True), II (True), III (False), IV (True)
- (C)I (False), II (False), III (True), IV (False)
- (D)I (False), II (True), III (True), IV (False)
Answer: (A) I True, II True, III False, IV False Official key: A
- Strain compatibility (IS 456 Cl. 38.1): when the concrete reaches , the steel strain is . Design yield strain of Fe415: .
- Balanced depth: (code: 0.48). At this depth both strains are reached at the same instant, so IV is False.
- Over-reinforced (): when concrete crushes, so concrete fails first. I is True.
- Under-reinforced (): steel yields before the concrete reaches 0.0035. II is True.
- Over-reinforced beams fail suddenly by crushing with no warning, so the code caps at . III is False.
- Answer: (A)
Trap: (B) marks IV True. In a balanced section neither material "wins"; crushing and yielding coincide.
Every RC beam design sheet and the ETABS/STAAD concrete design module checks first; if it fails, the designer deepens the section or adds compression steel rather than accept an over-reinforced, brittle beam.
Strains in concrete and steel of a balanced M20/Fe415 beam section at ultimate state as per IS 456
A singly reinforced concrete beam of balanced section is made of M20 grade concrete and Fe415 grade steel bars. The magnitudes of the maximum compressive strain in concrete and the tensile strain in the bars at ultimate state under flexure, as per IS 456: 2000 are ________ , respectively. (round off to four decimal places)
- (A)0.0035 and 0.0038
- (B)0.0020 and 0.0018
- (C)0.0035 and 0.0041
- (D)0.0020 and 0.0031
Answer: (A) 0.0035 and 0.0038 Official key: A
- IS 456 Cl. 38.1(b): in flexure the maximum compressive strain at the extreme concrete fibre is , whatever the grade of concrete.
- A balanced section is one where the steel just reaches its design yield strain when the concrete reaches 0.0035. For HYSD bars IS 456 Cl. 38.1(f) sets that strain as (elastic part plus the 0.2 % proof-strain offset).
- Check: , the familiar Fe415 limit in the note to Cl. 38.1.
- Answer: (A) 0.0035 and 0.0038
Trap: (C) comes from , i.e. forgetting the 0.87 (material factor 1.15). (B) and (D) start from 0.002, which is the limiting strain for direct axial compression (Cl. 39.1(a)), not bending.
These two strain limits are what every RC design program (ETABS, STAAD.Pro, RCDC) and the SP 16 design charts use to build the strain-compatibility check of a beam; a steel strain above 0.0038 at collapse is the proof that a Fe415 section is under-reinforced and will fail in a ductile way.
Can compression steel of Fe250 or Fe500 bars reach 0.87fy in a doubly reinforced beam as per IS 456?
Consider a doubly reinforced RCC beam with the option of using either Fe250 plain bars or Fe500 deformed bars in the compression zone. The modulus of elasticity of steel is N/mm2. As per IS456:2000, in which type(s) of the bars, the stress in the compression steel () can reach the design strength () at the limit state of collapse?
- (A)Fe250 plain bars only
- (B)Fe500 deformed bars only
- (C)Both Fe250 plain bars and Fe500 deformed bars
- (D)Neither Fe250 plain bars nor Fe500 deformed bars
Answer: (A) Fe250 plain bars only Official key: A
- At collapse the extreme concrete fibre is at 0.0035 (IS 456 Cl. 38.1(b)). Compression bars sit a distance below it, so by plane sections .
- Fe250 mild steel has a definite yield point (IS 456 Fig. 23B): is reached at , which is below 0.0035. It yields whenever , true for any practical beam.
- Fe500 deformed (cold-worked) bars follow Fig. 23A: is reached only at . Even a bar at the extreme fibre gets only about from the Fig. 23A curve, less than .
- Answer: (A) Fe250 plain bars only
Trap: (C) assumes compression steel always yields as tension steel does. For HYSD bars the code makes you read from the stress-strain curve (SP 16 Table F); only for mild steel does hold.
This is why design aids (SP 16 Table F) and software such as ETABS or RCDC compute for Fe415/Fe500 compression bars from strain compatibility instead of using ; assuming yield would overstate the compression-steel force and the moment capacity of doubly reinforced beams.
Ultimate moment of resistance of a singly reinforced cantilever beam, M25/Fe415, three 28 mm bars
Consider the singly reinforced section of a cantilever concrete beam under bending, as shown in the figure (M25 grade concrete, Fe415 grade steel). The stress block parameters for the section at ultimate limit state, as per IS 456: 2000 notations, are given. The ultimate moment of resistance for the section by the Limit State Method is ________ kN.m (round off to one decimal place).
[Note: Here, is the total area of tension steel bars, is the width of the section, is the effective depth of the bars, is the characteristic compressive cube strength of concrete, is the yield stress of steel, and is the depth of neutral axis.]
Answer: Official key: 295.0 to 305.0
- In a cantilever the tension is at the top, so the bars are at the top and the compression block at the bottom. ; .
- Force equilibrium : .
- Check (IS 456 Cl. 38.1, note): , so the section is under-reinforced and the steel yields, as the stress diagram assumes.
- Moment of the steel force about the compression force (Annex G-1.1(b)):
Trap: taking as the overall depth 600 mm gives , outside the key; the 45 mm is the effective cover, measured to the bar centres.
Cantilever balconies, chajjas and canopy beams fail on site when the top bars are trodden down during the pour; engineers rerun exactly this calculation with the reduced effective depth measured on site to decide whether the member needs strengthening.
Balanced doubly reinforced section: which change in steel area makes it under-reinforced?
Consider a balanced doubly-reinforced concrete section. If the material and other sectional properties remain unchanged, for which of the following cases will the section becomes under-reinforced?
- (A)Area of tension reinforcement is increased.
- (B)Area of compression reinforcement is increased.
- (C)Area of tension reinforcement is decreased.
- (D)Area of compression reinforcement is decreased.
Answer: (B) and (C) Official key: B;C
- Balanced means the neutral axis sits exactly at the limiting depth, (IS 456 Cl. 38.1: for Fe415). Under-reinforced means .
- Force equilibrium (IS 456 Annex G-1.2): .
- Decrease : the tension force on the right falls, so the concrete block needs a smaller to balance it. : under-reinforced. (C) is correct.
- Increase : the compression steel takes a larger share of the same tension, so again the concrete needs a smaller . Under-reinforced. (B) is correct.
- (A) and (D) do the opposite: grows past and the section becomes over-reinforced.
Answer: (B) and (C).
Trap: ticking (A) because more steel feels safer. Extra tension steel without extra compression capacity pushes the neutral axis down and the section fails by concrete crushing, without warning.
When a beam's depth is fixed by architecture, designers in ETABS or STAAD.Pro add compression steel precisely to pull the neutral axis back under xu,max; the software flags a section as over-reinforced when added tension bars push it past the limit, and the fix is more Asc, not more Ast.
RC beam 300 x 700, 2000 mm2 steel, m = 12, top fibre strain 0.0004: what is the stress in the steel?
Answer: Official key: 125 to 127
- Effective depth . With the tension concrete cracked, the transformed section is the compression concrete plus the steel counted as of concrete (working stress assumptions, IS 456 Annex B-1.3).
- Neutral axis from equal first moments: , i.e. , so .
- Plane sections remain plane, so strain is linear in depth: .
- Steel is elastic: , so the answer is .
- Check: , top-fibre stress , and gives the same value.
Trap: taking the steel strain equal to the top-fibre strain gives . The steel sits 398 mm below the neutral axis, farther than the top fibre is above it, so its strain is larger.
This cracked-section calculation is the core of serviceability checks: the steel stress under service load drives the crack-width estimate of IS 456 Annex F and is the governing limit for water-retaining structures to IS 3370. Design tools such as RCDC and ETABS report it in their crack-width checks of beams and slabs.
RC beam 350 x 600, 800 mm2 steel, M20/Fe415, IS block replaced by equal-area rectangle: what is Mu?
- (A)170
- (B)148
- (C)125
- (D)102
Answer: (B) 148 Official key: B
- . Steel force at collapse: .
- The IS 456 block has area per unit width, so . This is below (Cl. 38.1, Fe415): under-reinforced, the steel yields.
- Equivalent rectangle with the same stress and the same area: depth , so its force acts at from the top.
- , which is : option (B), 148.
The real IS 456 block puts the force at instead of , giving : the change in shape hardly matters. Trap: using the overall depth 600 mm as the lever arm base gives 160 kN.m, which is not an option.
Codes such as Eurocode 2 and ACI 318 use exactly this kind of equivalent rectangular block for hand design, and design software lets you pick the block shape; this question shows why the choice barely changes the beam capacity. Checking that (a ductile, under-reinforced beam) is the first line of every beam design sheet.
Fe500/M25 beam with neutral axis at 302 mm and xu,max/d = 0.456: what is the most probable mode of failure?
A rectangular singly reinforced concrete beam has a width of 300 mm and an effective depth of 550 mm. The grades of steel and concrete are Fe500 and M25, respectively. The area of steel in tension is 1963 mm2. The depth of neutral axis is 302 mm. The ratio of the limiting depth of the neutral axis () to the effective depth (d) of the beam is 0.456.
The most probable mode of failure of the beam is
- (A)compression failure
- (B)bond failure
- (C)shear failure
- (D)ductile failure
Answer: (A) compression failure Official key: A
- IS 456 Cl. 38.1: concrete crushes at a strain of 0.0035, and Fe500 steel counts as yielded at . That gives , the 0.456 in the question.
- Limiting depth: . Actual , so the beam is over-reinforced. The IS 456 stress block agrees: .
- When the concrete reaches 0.0035 the steel strain is only . The steel has not yielded, so the concrete crushes suddenly with little warning: (A) compression failure.
Trap: (D) ductile failure is the under-reinforced case (), where the steel yields first and the beam cracks and sags visibly before collapse. That is the behaviour IS 456 wants, and the reason it caps at .
ETABS and STAAD.Pro RC design modules check for every beam. When it exceeds the limit they either report the section as over-reinforced or switch to a doubly reinforced design, and a checking engineer reviewing hand calculations looks at this ratio first.