Lesson finished
Unlock all 6 lessons of Basics of PlasticsFull course ₹40,000 · paid
Machine Tonnage, DFM Part Review and Injection Molding Defects
A free lesson from Skill-Lync's Basics of Plastics course, on Grow by Skill-Lync · Last updated 16 Nov 2026 · Session: “Week 3”
What will you learn in this free Basics of Plastics lesson?
The lesson shows how clamping force is chosen for an injection molding machine and calculated from projected area and injection pressure. It then covers the points a DFM team reviews before mold design and defects such as hesitation, overpacking and unbalanced flow.
- Calculating machine tonnage from projected area
- Problems from too high or too low clamping force
- Part details checked during DFM review
- Defects like gloss difference, hesitation and overpacking
What comes after lesson 3?
Later in Skill-Lync's Basics of Plastics course (paid): lesson 4, Week 4; lesson 5, Week 5; lesson 6, Week 6. The full course has 6 lessons (2 h 31 min of video); see the course overview or its price and syllabus.
Lesson transcript
Machine transcript of the lesson audio (lightly cleaned). Technical terms may contain errors; the video is the reference.
Hello guys, hope you are doing good. Welcome back to another session of Basics of Plastics. In the previous session, we learned about product development process, departments related to mold manufacturing industries, parts and types of mold and few basics of draft and parting line. In this session, we will be learning about machine tonnage which will be a very short topic and then we will mainly focus on the entire review process of plastic parts done during DFM and then we will be covering the defects that can occur during the mold design process.
So, now let us look at the concept of tonnage of the injection molding machine. The pressure with which the molded material is injected in the injection molding machines is very high. In most of the products, the injection pressure is around 4 to 5 tons per square inch. In some cases, it can be much higher than this too. So, to ensure that the core and cavity do not get separated due to this high injection pressure, we have to provide proper clamping for the mold. The amount of clamping force provided by the clamping mechanism is decided by the tonnage of the machine.
So, for example, if we have a 100 tonnage machine, then that basically means that 100 tons of clamping force is provided by the clamping mechanism. Now, it is probably easy to imagine why we cannot have a low or very low clamping force. The tonnage of the machine selected is very less. The core and cavity will get separated when the material is injected and result in flashes. However, again, we also can't use machines with very high tonnage values. If the clamping force for the mold is too high, then it can again cause defects like burns, short shots and glass differences.
Also, a very high clamping force can damage the venting system, inserts and also the core and the cavity block. So, the selection of right tonnage of a machine is also very important. The clamping force can't be kept too high or too low as both of these will cause issues. This force should be within a certain range to ensure proper injection molding process. So, the tonnage of the machine is calculated based on a formula, which is projected area multiplied by injection pressure divided by 1000, where the projected area is in centimeter square and injection pressure is in kilogram per centimeter square.
Projected area is the projected surface of the entire model along the tooling direction. Tooling direction is the direction along which your mold is oriented and your core and your component will be moving. So, let's say the projected area we found was about some 35 centimeter square and the injection pressure if we use ABS material would be around 500 kilometer per centimeter square. So, we will multiply 35 by 500 which will be 17,500 and then divide by 1000 which will give you the value of 17.5. So, basically 17.5 tons of clamping force will be required for this machine.
But the machines available in the industry comes in specific sizes. So, a 17.5 tonnage machine might not be available and in that case you will select the closest value of the machine higher than this calculated value. For example, if you have a 15 tonnage and 20 tonnage machine available, then you will go for a 20 tonnage machine. In this section, we will look at DFM in a bit more detail. If you remember, I had covered DFM briefly when we were discussing the departments in mold manufacturing industries.
We know that DFM stands for Design for Manufacturing. So, basically, the DFM receives the plastic component for which the mold is required by the customers or the product design team. The review of the product is done by the DFM team in terms of the design, manufacturing and the molding aspects and they also check if all the data is available to proceed with the tool design. If they think there may be some problems in creating the mold for the given product, then they convey that to the customers or the product design team.
Here, I have mentioned the checklist which is followed by the DFM team to ensure that they have all the inputs required for designing the mold. And I will also be explaining each point in detail in the next few slides. So, first, we will be covering part details. The first point is shrinkage. Whenever the mold and material in the mold solidifies, it shrinks. So, the actual part size obtained is less than the size of the mold. You know that plastic, when it is cooled down, it shrinks, right?
So, the same case happened here. So, the size of the mold is designed in such a way that it takes into account the shrinkage of plastic and it gives a part with correct dimensions. To do that, we need the extract shrinkage value for the material that is being injected into the mold. The next point is material. The material here refers to the plastic material for which we make the component. And the next is the number of cavities. The number of cavities required is also asked from the customers.
The DFM team can make suggestions for it. But the final decision comes from the customer side. And the next point is inlet type. There are different types of gates used. And depending on what type of gates you use, there may be some marks on the final product. So, the customers are earlier informed on what are the effects of using specific types of gates. And depending on the requirement, the gate type is selected. Types of gates will be covered in detail in a separate session. The next one is surface demands.
So, the type of surface finish required is also asked to the customers. Whether they want the surface to have a textured finish or a glossy finish, it all depends on their demand. If the part manufactured won't be visible from outside, then there won't be any need for polishing the tools and providing a good surface finish. For example, if you are watching this video on a PC, then you probably have a keyboard in front of you. Now, if you open your keyboard, then you will find many plastic parts inside it.
Now, since these parts are not visible from outside, it doesn't matter what surface finish it has. Adding good surface finish requires additional cost and time and must be avoided where it's not necessary. Also, the type of surface finish required will also affect the draft angle given for the geometry. Last point is if there is any engraving required. For example, you may see the company logo engraving on many products. So, if it is required, then the details regarding the engraving is also taken from the customers. Even in these engravings, for the length and width of engravings, there are some standards to be followed.
That's because these engravings are milled by CNC machines. So, based on the size of the cutters that are available, there are standard sizes for the engravings. So, next we will see parting surface. Parting surface is the surface that splits the core and cavity. In most of the products manufactured by injection molding, you can see a visible mark along the parting surface. So, the customers are informed that there will be a mark here and they will also be asked if it is fine or should we change the parting surface, all these things.
So, on the diagram to the left, you can see that the parting surface marked in white arrows. So, this is kind of a cap. And even when using sliders, there is a visible mark along the parting line of the product. Also, we have not covered the topic of sliders yet. We have a separate topic on sliders where I will be explaining how sliders work in detail. For now, just know that there are some cases where the core and cavity is not enough for creating a proper mold.
And that sliders are added along with core and cavity to create a proper mold. And these sliders will also leave a mark similar to the parting line. So, we have to inform the customers that there will be a mark present along this line. So, here in the right side image, you can also see a split line, which is the mark because of the use of sliders. So, here this is a B pillar lower drum. So, this is a pillar which is used in automotive vehicles. To be precise, cars.
Here also, you can see a red color parting line. Next, for injection molded parts, there is a visible gate mark present. Most of the time, the location of the gate is placed where it won't be visible from outside. But in case it is visible from the outside, the customers are also informed about these marks. You can find these gate marks on the bottom of buckets, pens, bottles and many other household injection molded products. Also, we should note that in some of these products like buckets tables, you know, plastic tables, we cannot simply cover the gate marks because they are not closed products.
They are open products. So, obviously, these marks will be visible. Next, we will go to wall thickness. For the plastic components manufactured, we try to keep the overall thickness relatively constant. This is because if there is a variation in the thickness of the component, it will lead to a non-uniform shrinkage of material as thick sections shrink more than the thinner sections. This non-uniform shrinkage causes the component manufacture to warp. In the diagram, you can see that more warp age was observed when there was a higher change in the thickness of sections.
However, we cored out the thicker region, which basically means that we make it hollow, then warp age can be avoided. Coring out can also make parts weaker. So, sometimes rips are added in the cored out sections. And usually, the thickness values for components vary from 0.6 to 5 mm. If we try to make parts lower than 0.6 mm thickness, then there won't be a proper filling of material in the mold. The material itself will solidify before reaching the ends. This defect also has a name. It is called a short shot.
Details regarding the defect in injection molding will be covered later in the same session. Right now, we will look on what we are going through. For thickness values higher than 5 mm, gas-assisted injection molding is used. If there is a sorry offset in the root of previous For deeper holes in a part, then we have to use longer core pins to make the deep hole. But using longer pins from the core side results in heat dissipation problems. If heat dissipation does not take place properly, then it will lead to burn marks in the hole region, which is a type of defect again.
As a rule of thumb, if the length of the hole is greater than 7 times the diameter of the hole, then hole would be considered too deep. To counteract, we split the hole in the two parts. So, some part of the hole is made using the cavity side and the rest of the hole is captured from the core side. This will help to reduce the length of the core pin used. Another point to note is that in general, we try to avoid features in the cavity side.
This is because creating these pins for holes in the cavity side creates more surface in the cavity side where the material can stick. Sticking off material in the core side is not as big as an issue like how it is as big in the cavity side. Because on the core side, we have ejector pins to eject the pad which is not available on the cavity side. So, that is why we make the pins for capturing holes from the core side. And if the length is too large, then we also make a pin from the cavity side if it is required.
So, now this is like a short or brief explanation on tolerance. When we have the same upper and lower limit for tolerance, for example, 10 plus and minus 1. So, this means that the dimension of the component can be between 9 and 11. And we see that both the numbers are equally spaced from 10. So, this would be a case of symmetric tolerance. But if we don't have the same limits, for example, 10 plus 1 minus 0.5. Now, the dimension has to be between 9.5 and 11.
In such cases, there is a possibility that due to shrinkage, the dimension of the part may go below 9.5. So, again, in such cases, mold is designed for a dimension of 10.25, which is the average of 9.5 and 11 to ensure that the dimension is within the tolerance. When we close the mold, some air is trapped between the surface. Due to the strapped air, the molten material can't fill the entire mold region and some defects will be found in the finished product. To avoid these, some channels are provided in the mold to allow the air to escape.
This process of providing air channels to remove the trapped air is called as venting. Next, we will see ejector pads. But before we see ejector pads, I will show you what problems might occur while ejecting components with low thickness. So, in the diagram, you can see that the thickness of the highlighted feature is 1.4 mm, which is the yellow color highlighted feature. However, the ejector pins come in standard sizes of 3 mm or 6 mm. So, if we try to eject the component from this region, then that won't be possible because the ejector pin of higher thickness can't move through the port.
In the specific case, this issue can be avoided by providing ejector pins at some other place. But that might not be the case in all situations and to deal with such situations, ejector pad is one solution we can use. In this video, if you can see there is an ejection pin or ejector pin, then there is a core and then there is a component. Now, you can see there is a ejector pad given here. For example, if this ejector pin is 3 mm and the wall thickness of this component is 2 mm and assuming the ejector pad is not given, obviously, we will have 1 mm difference in the outside.
So, to negate this difference and give a proper ejection, we give a ejector pad which is again 3 mm of diameter. And using this, we try to eject the component. So, if you can see in this video, the ejection is done like this. This would be a good time to explain the concept of undercuts in molding. Undercuts are those features in the part due to which the part cannot be directly ejected from the mold. If you see this right side figure, the top part is the core and the bottom part is the cavity.
Once the material solidifies, you will notice that it is not possible to eject the part from the core due to highlighted section. This feature is called the undercut. Now, there are two types of undercut available, internal undercut and external undercut. The diagram which you see on the left side is the internal undercut and the right side is the external undercut. To deal with external undercut, we use side cores or sliders. So, as I already mentioned, side core or sliders will be a separate topic and I will be explaining it later.
Here, the diagram which you are seeing is an insert. In this image, the desired product is a screwdriver. We know that the working part of a screwdriver is metal and the handle is almost always a plastic handle. But as the metallic part is fixed inside the plastic part using shoulders, it is common to have undercut inside the plastic part. So, to overcome this fixing difficulty, the working metal is used as an insert for the plastic part. The red arrow shows us the location of the undercut.
So, next we have a diagram which is showing ejector inserts. Let us assume we have a part with a large flat surface. Let us say for 500 mm or something. So, in this case, instead of providing multiple ejection pins to eject the part out, we can use an ejector insert for the ejection of the plate. In the given figure, this orange color is the ejector insert. The ejected part will be the blue color part. So, the green part is the ejection pin. So, this insert helps in distributing the ejection force over a large surface without the need of providing extra ejection pins.
Ejector inserts can also be used in cases where the customer does not want any ejector pin marks on the part. So, in that case, an ejector insert covering a large area of the part can be used in which or which will help avoid the marks that would have been left if multiple smaller surfaces or surface area ejector pins were used. So, in the last session, we saw the function of the guide pillar and its role in the overall molding operation. The left side is the core side in this picture which you are seeing and the right side is the cavity side.
The guide pillar is used for aligning the core and cavity. You can see that there is a projection on the cavity side which is called the guide cone. This is basically for interlocking the cavity and core region. Again, in the last session, I had mentioned that the core plate thickness is always kept more than the cavity plate as there is a chance of deformation of the core plate due to hot injected material. The pressure of the injected material may be around 600 to 700 bars and to avoid any chance of deformation of the core plate, an additional support block is placed between the core plate and bottom moving plate of the mold.
Now, you might ask, why can't we just keep increasing the thickness of the core plate? What is the need for a support block? It is true that the deformation problem can always be solved by increasing thickness but there is a limit up to which increasing the thickness is cost effective. This is because when we increase the thickness, we have the increased material cost for core plate and then the length of the holes which need to be milled in the core plate for the ejection pin will also keep increasing.
So, this is why we use a support block instead. So, there are two types of cutters used for machining, the ball nose cutter and the flat cutter. Ball nose cutters are used for 3D profiles. So, if a parting line is along a 3D surface, then we need to make a 3D profile that would require more time. So, that is also one of the reasons we try to make the parting line in the same plane. When we use ball cutters for machining sharp corners, it produces a fillet at the corner as you can see on the right side.
The creation of this fillet makes it difficult to match the core and the cavity side. So, that is why some relief is provided near sharp corners in the mating surface. In some cases, if the length of the rib is very long, then it gets difficult to eject the rib from the mold because the plastic sticks to the walls of the cavity. For such cases, we make use of free play inserts. In the first diagram, you see the cavity region and the part formed within it through injection molding.
Now, if the length of this rib is more, then it would be more difficult to eject it out of the mold. In such cases, a free play insert is added. So, the purple section you see in the diagram is the free play insert. The free play insert is present in the cavity section. When the material is formed through injection molding, a screw which you see at the top drives the free play so that it goes downwards direction which in turn pushes the part out of the cavity.
Next, we will see multi-gate position for a long part. The length of the plastic part manufactured is more. Then we provide multi-gates for the part. The exact length after which we need to provide an additional gate depends on a material property called flow length. Flow length is the distance after which the molten material will solidify. So, for example, in the below diagram, let us assume the length of the part to be around 1500 mm. And let us say we know that for the given valve thickness, the flow length is 250 mm.
So, here since the length of part is more than the flow length, we will have to provide additional gates. So, if we think of providing 8 additional gates, we can check that 1500. The total length divided by 8 would be given some value between 180 to 190, if I am not wrong. And since this value would be less than the flow length of the material, there should not be any freezing of material due to an inadequate number of gates. So, this is how the number of gates is selected based on the flow length of the material.
Now, we will look at the concept of balancing the mold block. The pressure of the injected material in the mold is very high and proper clamping needs to be provided to ensure that proper injection molding takes place. Remember, I mentioned earlier that we select a specific tonnage of machine that decides the clamping force acting on the machine. This clamping exerts an equal amount of force at all the ends of the machine. So, the diagram which you see on the left is the side view of the mold.
You can see the runner. The cavity. And the mold block. In this image, the runner is kind of exaggerated, but usually it is tapered as the tip reaches the part. And on the right, you can see the same mold block in an isometric view. In the first case, you can see the runner is at the center of the mold. So, when the molten material is injected into the mold, there will be a force at the center of the mold block, which will try to separate the mold block from each other.
This force is denoted by the letter F in the diagram. And since we don't want the mold blocks to get separated, an equal clamping force will be exerted equally from all ends to counteract the pressure of molten plastic. This clamping force is represented by the letter P and the value for this will be calculated based on the formula for calculating the tonnage of the machine. So, since the opposing force at the center is balanced by the clamping force at the ends, the first mold is said to be balanced and will function properly.
Now, let's look at the second case. Let's say we can't provide the gate location at the top and we have to provide the gate location at some other face. So, if you provide the runner as shown in the second diagram or in the left side, I mean the left side diagram of this slide, then the point at which the injected material creates an opposing force will also change and it will be near the ends as shown in the right side diagram. And since it is not possible to have different clamping forces at each end, there will be some points in the mold where the clamping force is too high or too low and we can't have either of these cases.
So, this is called an unbalanced mold and we can't use this. So, what else can we do to keep the mold balanced and also have the gate location at the same point as the same, you know, second case. In the third case, you can see that the size of the mold block itself is increased in order to keep the sprue at the center. So, in this case, the molten material injected will exert an equal force and all the ends and the clamping force will also exert a constant equal force force at all ends to counteract this force and the mold will also be balanced in this case.
But imagine we only have a right side mold and there is no left side mold. Then again, there will be imbalance. So, now instead of case 3 which only had right, we will again have a left side mold and now it seems to be balanced. So, the thing to note here is that the sprue location should always be at the center of the mold. For single cavity tools, we try to go for case 1 as it is balanced and the material cost and runner length is also less in case 1.
But in case, we can't go for case 1 due to gate location constraints, then we can go for case 3. In the case of multi-cavity tools, we always go for case 3. Here, you can add a second cavity to the same mold and have a two-cavity mold. So, if we have a part with a slot in the center like this part for example, we can place the gate location at the center of the part as shown by the blue arrow in the diagram. Instead of outside the part.
So, here outside the part would be the red arrow. The blue arrow case is similar to case 1 which we saw in balancing and the red arrow is similar to case 3 which we saw in balancing. So, providing the inlet from the center will reduce the runner channel length and help in reducing costs of runner channels and also reduce material wastage. There is another point to note which is that generally a better surface finish will be given on the cavity side compared to the core side.
Also, the draft angles on the cavity side and core side depends on the part to be manufactured. This is done to ensure that the plastic does not stick to the walls. Also, if you remember the working of the mold, I had mentioned that the cavity side is fixed and the core side is moving for the two-plate mold. So, when the core moves away from the cavity after the part is formed, the part should come along with the core where it is ejected using ejector pins. The part should not stick to the cavity walls when the core plate moves back.
So, to ensure that the part does not stick to the cavity, better surface finish and higher drafts are given on the cavity side. So, here in this diagram, the polished grain 320 and medium glass blast are types of surface finish. Polished grain finish is a better finish compared to the glass blast. The right side arrow marks are given for the drafts. Next, in this diagram shown, if you provide the gate location at the center, like how it is shown in the left side diagram with a green block, you can see that some regions of the mold will fill earlier compared to the other regions.
The wall region nearest to the gate will be filled first and the region farthest from the gate will fill last. By nearest and farthest in this left side diagram, I mean flow path 1 is going to be filled faster than flow path 2. But what if we want a uniform flow over the part to achieve that? We can use or, you know, make use of something called flow leaders. So, flow leaders are the specific regions that are purposefully made thicker to promote the flow of material.
In our case, the flow path 1 is made thinner and the flow path 2 is made thicker. Another problem which we might face is the formation of air pockets like how it is given in the right side diagram. So, this is also again due to fast and slow flow of material in the same part. To avoid this, again we can use flow leaders or flow restrictors in some cases. So, now we will be looking at some of the defects which can occur in the molding process.
Here all the defects are mentioned that I will be covering in this section. So, we shot short, slash, weld lines, sink marks, blisters, jetting, burn marks, walk page, gloss differences, hesitation, over packing and unbalanced flow. So, the first one look we are looking is at the short, short, the short, short is like to acquire a component with correct dimensions. The molten material must completely fill the cavity region, but in some cases this does not happen. In the diagram you can see that there are some regions where the flow of material did not take place.
So, what you see here is the short, short, a short, short is the incomplete filling of a mold cavity which results in the production of an incomplete part. Now, this can happen due to number of reasons. It is possible that the amount of material injected into this mold itself is not sufficient to fill the entire mold. It is also possible that the pressure of the injected material is not sufficient to flow through the entire cavity. If proper vents are not provided, then the air would be trapped in some regions and the material might not be able to fill it.
Also, if the size of the gates is very small or in regions with thin cross sections, the material may freeze before filling the entire cavity region resulting in a short, short. Flash is the excess material that you will find attached to your component. Now, this can happen when the core and cavity plate do not close properly or the injection pressure is too high and the material seeps outside the mold. To fix this issue, we have to do some post-processing operations which will increase the production time.
Next, we will see about weld lines. When two molten material flow fronts meet at a specific point, it creates a visible partition in the surface. This defect is known as a weld line. The component is especially weaker in the weld line and will easily break if force is applied along the weld line. In the diagram here, you can see how the weld lines are formed by changing the position and number of gates. In the second diagram, you can see there are four gates used and this leads to creation of four weld lines.
Now, since weld line is a type of defect which makes the component weaker, the case 2 is better than case 1. This is because the component will be a lot weaker along the single weld line in the first case compared to the weld lines in the second case. This weld line which is formed in the first case is called a weak weld line and whichever is formed in the second case are called strong weld lines. In case 3, you see that the position of the gate was changed so that no weld line would be formed.
So, as far as the strength of the component is considered, case 3 provides the best ever component. However, due to customer requirements, it might not be able to, you know, provide case 3 for every component. So, that time we try to go to the four weld line case which is the second case. Now, we look at sink marks. Sometimes, due to the shrinkage of the material at areas with higher thickness, a small crater or depression is formed. So, the customers are informed of any possible sink marks that may appear due to current dimension of the product.
We usually see these defects around the ribs. The rib thickness is usually kept around 0.5 to 0.7 times thickness of the part to reduce sink marks. Next, we will see blisters. Sometimes, during the mold process, air may be trapped between the molten material which will result in the formation of blisters. It is also possible that the feed material used is not dry enough and while heating the material, it results in the formation of steam, creating pockets of trapped air. Again, blisters affect the component's aesthetics and also weakens the component.
Next, we look at jetting. When the molten material is passed through the gate with a very high pressure. It is sometimes possible that instead of uniformly filling the cavity section, the flow will have a wavy snake-like pattern which you see here. This is not a desirable way of molten material filling the cavity as this leads to weak parts and also many internal defects. So if we have a case where jetting may occur, then we can either increase the gate area or change the position of the gate as you see in this diagram.
So due to this, more uniform flow occurs throughout the cavity. Here, as the material flows through the runner and the gate, due to the position of the gate, the material will completely fill the left region before moving on to the right part and thus a more uniform flow will be achieved. Whether a change in the gate location will be needed or not to prevent jetting is usually found by mold flow analysis and then the mold designer has to design the gate accordingly. So next we will see burn marks.
In the injection molded products, you will sometimes notice a charred or burnt dark, you know, plastic region. This is called a burn mark. This can happen when the temperature of the molten material injected is very high. Burn marks can also occur when the air trapped in the cavity overheats instead of escaping out of the system. So controlling the temperature of molten material and providing proper venting usually fixes this defect. Next we will see warpage. So warpage is a defect in which the shape of the component deviates from the required shape.
Earlier slide, we also saw warpage which can be, you know, cured with hollow surfaces. So that is what is continuing here. This happens when there is a uneven shrinkage of material which occurs due to uneven cooling of the material in the mold. There can be many reasons due to which warpage occurs. One of the reasons is non-uniform wall thickness in the cavity or improper cooling channels. Next in injection molded parts, you will sometimes notice that some regions have a better surface finish compared to other regions.
This results in a visible gloss difference in the product. So this can happen due to improper surface finish of the mold tool itself or it can also occur due to shrinkage differences or there might be even an issue with the raw material being used. Next hesitation. Hesitation is a defect in which the flow of material along a specific direction slows down or completely stops. In case 1, which is the first one, the left side case, you can see that the rib section is not being filled.
This is because of the flow of the or the flow direction of the material. You can see how the rib is perpendicular to the flow direction. But in the second, you know, case, the rib is completely filled because the flow direction, the material flow direction is parallel to the axis of the rib placed. So these kind of defects can be avoided with such changes of flow direction. Next, we will see overpacking overpacking is a defect in which more material is concentrated in specific regions compared to other areas.
The diagram below, you can see that due to the positioning of the gate, more material is being concentrated on the left side compared to the right side of the part. This will result in non-uniform shrinkage of the material and also non-uniform density in the overall part. Next, the selection of the right gate or right gate location should solve the issue of overpacking. Next comes unbalanced flow. We say that the flow is unbalanced when some extremities of the mold filled is earlier compared to others. If all the ends fill at the same time, then it is called balanced flow.
Unbalanced flow can again result in many issues such as work page density differences and higher cycle time. Unbalanced flow can also give loss difference in the part. So again, flow leaders which I mentioned in the previous section can be used to acquire a more balanced flow throughout the mold. So in this session, we learned about the machine tonnage. We saw the points that are taken into consideration by the DFM team before starting the mold design. And we also took a brief look at defects which can occur during the molding process.
And that is it for this session. Thank you for watching the video.